Ürün Kodu : 1518 Marka : TurkishStocks
GLASS EDGE PROCESSING BEVELLING It is the process of polishing the glass edge at 90 ° and the front edge of the glass at the desired angle. Bevel width varies with angle. CHANNEL OPENING Engraving the surface of the glass along a line at a depth of 2 mm is called shaping. RODAJE It is the process of polishing glass edges and corners. Glass rim and belt receiving the sharpness of the corner processing run in, 90 ° and 45 ° angle with the polishing of the flat grinding, while the polishing of the
 GLASS EDGE PROCESSING
BEVELLING
 It is the process of polishing the glass edge at 90 ° and the front edge of the glass at the desired angle. Bevel width varies with angle.
PRODUCTION LIMITS
 MAX: 2000 x 2500 mm, MIN: 150 x 150 mm
 CHANNEL OPENING
 Engraving the surface of the glass along a line at a depth of 2 mm is called shaping.
RODAJE
 It is the process of polishing glass edges and corners. The process of removing the sharpness of the edges and corners of the glass is called band lapping, the polishing process with 90 ° and 45 ° gradients, flat lapping, arc lapping, and lapping gradually, profile lapping. Polishing is the polishing of the matting cutting surface after grinding in a second process.
PRODUCTION LIMITS
 MAX: 2600 x 4000 mm, MIN: 300 x 300 mm
 
                         
                                    